Plastic steel

United States "TORMOST"


DC-425 (maste)


DC-426 (semi-mushy)


DC-427 (for stainless steel and aluminum)


  • Product uses:

    Metal and cement castings that remedy defective or construction errors can be remedied regardless of size or fine cracks.


    Product usage:

    1.First, wipe the surface or the surface of the impurities or oil stains to clean, in order to enhance the bonding strength of plastic steel.

    2.Blending ratio: according to the volume agent --- 3 parts of plastic steel with 1 part of hardener.

    3.The blending treatment is carried out at a normal temperature of 25 ° C for 30 minutes, and it takes 24 hours to completely harden. The color is dark gray after the hardening and the temperature is up to 250 F.

    4.How to use DC-427: After the agent is blended, the surface is hardened at a temperature of 25 ° C for 20 minutes to 30 minutes, and it takes 16 hours to completely harden.


    Note:

    1.If it touches the skin, rinse it off with soap and water.

    2.If you accidentally touch your eyes, wash them with plenty of water immediately. If necessary, please call a doctor.